Reasons why non-woven fabrics cannot be reused

Sterile barrier properties are lost after use

According to research, the shelf life of sterile items is closely related to the thickness of the non-woven fabric and the number of layers of wrapping cloth. After a series of high-temperature steam sterilization and chemical washing of disposable non-woven packaging materials, the fiber structure is deformed, the holes are sparse, the thickness is reduced, and even small holes that are not easily detectable by the naked eye appear, and the bacteria resistance rate will drop suddenly or Loss of bacteriostatic properties. The requirements for packaging materials in the "Technical Specification for Disinfection" are: in the storage process, provide a bacterial barrier and maintain a sterile state. If the disposable packaging material is used repeatedly to package the device, the sterilized storage cannot reach the safe expiration date.

Internal microscopic properties change after sterilization

Non-woven packaging materials are generally SMS composite non-woven fabrics. The main material of this type of non-woven fabric is polypropylene, which is processed through multiple processes through meltblown and spunbond processes. The microstructure is fine plastic fibers (see the figure below). Shrinkage after being exposed to high temperature is a characteristic of plastic items. There is no real high temperature resistant plastic, and high temperature resistance is also a relative concept. Therefore, non-woven fabrics will also have corresponding shrinkage reactions on the microscopic level. 


You Might Also Like

Send Inquiry